Er Inconel 600 et rustfritt stål?
Inconel komposisjon
| Inconel | Element (% etter masse) | ||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Ni | Cr | Fe | Mo | NB | Co | Mn | Cu | Al | Ti | Si | C | S | P | B | |
| 600 | 72.0 | 14.0–17.0 | 6.0–10.0 | 1.0 | 0.5 | 0.5 | 0.15 | 0.015 | |||||||
| 617 | 44.2–56.0 | 20.0–24.0 | 3.0 | 8.0–10.0 | 10.0–15.0 | 0.5 | 0.5 | 0.8–1.5 | 0.6 | 0.5 | 0.15 | 0.015 | 0.015 | 0.006 | |
| 625 | 58.0 | 20.0–23.0 | 5.0 | 8.0–10.0 | 3.15–4.15 | 1.0 | 0.5 | 0.4 | 0.4 | 0.5 | 0.1 | 0.015 | 0.015 | ||
| 690 | 59.5 | 30 | 9.2 | 0.35 | 0.01 | 0.02 | 0.35 | 0.019 | 0.003 | ||||||
| 718 | 50.0–55.0 | 17.0–21.0 | balansere | 2.8–3.3 | 4.75–5.5 | 1.0 | 0.35 | 0.2–0.8 | 0.65–1.15 | 0.3 | 0.35 | 0.08 | 0.015 | 0.015 | 0.006 |
| X-750 | 70.0 | 14.0–17.0 | 5.0–9.0 | 0.7–1.2 | 1.0 | 1.0 | 0.5 | 0.4–1.0 | 2.25–2.75 | 0.5 | 0.08 | 0.01 | |||


Inconel legeringer
Legeringer av inconel inkluderer:
Inconel 600: Solid løsning forsterket
Inconel 601
Inconel 625: Syrebestandig, god sveisbarhet. LCF-versjonen brukes vanligvis i belg.
Inconel 690: Lavt koboltinnhold for kjernefysiske applikasjoner, og lav resistivitet
Inconel 713C: Nedbørsherdbar nikkel-krombasert støpt legering
Inconel 718: Gamma double prime forsterket med god sveisbarhet
Inconel 751: Økt aluminiuminnhold for forbedret bruddstyrke i 1600 grader F-området
Inconel 792: Økt aluminiuminnhold for forbedrede høytemperaturkorrosjonsegenskaper, brukt spesielt i gassturbiner
Inconel Ekvivalente karakterer
| STANDARD | WERKSTOFF NR. | UNS | GOST | AFNOR | JIS | BS | EN | ELLER |
|---|---|---|---|---|---|---|---|---|
| Inconel 600 | 2.4816 | N06600 | МНЖМц 28-2,5-1,5 | NC15FE11M | NCF 600 | NA 13 | NiCr15Fe | ЭИ868 |
| Inconel 601 | 2.4851 | N06601 | XH60BT | NC23FeA | NCF 601 | NA 49 | NiCr23Fe | ЭИ868 |
| Inconel 617 | 2.4663 | N06617 | ||||||
| Inconel 625 | 2.4856 | N06625 | ХН75МБТЮ | NC22DNB4M | NCF 625 | NA 21 | NiCr22Mo9Nb | ЭИ602 |
| Inconel 690 | 2.4642 | N06690 | ||||||
| Inconel 718 | 2.4668 | N07718 | ||||||
| Inconel 725 | - | N07725 | ||||||
| Inconel X-750 | 2.4669 | N07750 |
Inconel smeltepunkt, tetthet og strekkstyrke
| Tetthet | Smeltepunkt | Strekkstyrke | Yield Strength (0.2%Offset) | Forlengelse | |
|---|---|---|---|---|---|
| 600 | 8,47 g/cm3 | 1413 grader (2580 grader F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
| 601 | 8,1 g/cm3 | 1411 grader (2571 grader F) | Psi – 80,000 , MPa – 550 | Psi – 30,000 , MPa – 205 | 30 % |
| 617 | 8,3 g/cm³ | 1363 grader | Større enn eller lik 485 MPa | Større enn eller lik 275 MPa | 25 % |
| 625 | 8,4 g/cm3 | 1350 grader (2460 grader F) | Psi – 135,000 , MPa – 930 | Psi – 75,000 , MPa – 517 | 42.5 % |
| 690 | 8,3 g/cm³ | 1363 grader | Større enn eller lik 485 MPa | Større enn eller lik 275 MPa | 25 % |
| 718 | 8,2 g/cm3 | 1350 grader (2460 grader F) | Psi – 135,000 , MPa – 930 | Psi – 70,000 , MPa – 482 | 45 % |
| 725 | 8,31 g/cm3 | 1271 grader -1343 grader | 1137 MPa | 827 MPa | 20 % |
| X-750 | 8,28 g/cm3 | 1430 grader | 1267 MPa | 868 MPa | 25 % |
Rustfritt stål
Rustfritt stål tilsvarende karakterer
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| SS 304 | 1.4301 | S30400 | SUS 304 | 304S31 | 08Х18Н10 | Z7CN18-09 | X5CrNi18-10 |
| SS 304L | 1.4306/1.4307 | S30403 | SUS 304L | 304S11 | 03Х18Н11 | Z3CN18-10 | X2CrNi18-9 / X2CrNi19-11 |
| SS 310 | 1.4845 | S31000 | - | - | - | - | - |
| SS 310S | 1.4845 | S31008 | SUS310S | - | 20Ch23N18 | - | X8CrNi25-21 |
| SS 316 | 1.4401 / 1.4436 | S31600 | SUS 316 | 316S31 / 316S33 | - | Z7CND17-11-02 | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 |
| SS 316L | 1.4404 / 1.4435 | S31603 | SUS 316L | 316S11 / 316S13 | 03Ch17N14M3 / 03Ch17N14M2 | Z3CND17-11-02 / Z3CND18-14-032 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 |
| SS 317 | 1.4449 | S31700 | SUS 317 | - | - | - | X6CrNiMo19-13-4 |
| SS 317L | 1.4438 | S31703 | SUS 317L | - | - | - | X2CrNiMo18154 |
| SS 321 | 1.4541 | S32100 | SUS 321 | - | 08Ch18N10T | - | X6CrNiTi18-10 |
| SS 321H | 1.4541 | S32109 | SUS 321H | - | - | - | X6CrNiTi18-10 |
| SS 347 | 1.4550 | S34700 | SUS 347 | - | 08Ch18N12B | - | X6CrNiNb18-10 |
| SS 347H | 1.4961 | S34709 | SUS 347H | - | - | - | X7CrNiNb18-10 |
| SS 446 | 1.4762 | S44600 | - | - | - | - | - |
Sammensetning av rustfritt stål
| Karakter | C | Mn | Si | P | S | Cr | Mo | Ni | N |
| SS 304 | 0.08 maks | 2 maks | 0.75 maks | 0.040 maks | 0.030 maks | 18 – 20 | - | 8 – 11 | - |
| SS 304L | 0.03 maks | 2 maks | 0.75 maks | 0.045 maks | 0.030 maks | 18 – 20 | - | 8 – 12 | 0.10 maks |
| SS 310 | 0.25 maks | 2 maks | 1,50 maks | 0.045 maks | 0.030 maks | 24 - 26 | - | 19 - 22 | - |
| SS 310S | 0.08 maks | 2 maks | 1,50 maks | 0.045 maks | 0.030 maks | 24 - 26 | - | 19 - 22 | - |
| SS 316 | 0.08 maks | 2 maks | 0.75 maks | 0.045 maks | 0.030 maks | 16 - 18 | 2 - 3 | 10 - 14 | 0.1 maks |
| SS 316L | 0.3 maks | 2 maks | 0.75 maks | 0.045 maks | 0.030 maks | 16 - 18 | 2 - 3 | 10 - 14 | 0.10 maks |
| SS 317 | 008 maks | 2 maks | 1 maks | 0.040 maks | 0.03 maks | 18 - 20 | 3 - 4 | 11 - 14 | 0.10 maks |
| SS 317L | 0.035 maks | 2 maks | 1 maks | 0.040 maks | 0.03 maks | 18 - 20 | 3 - 4 | 11 - 15 | - |
| SS 321 | 0.08 maks | 2 maks | 0.75 maks | 0.045 maks | 0.03 maks | 17 - 19 | 5xC min 0,60 % maks |
9 - 12 | 0.10 maks |
| SS 321H | 0.04 - 0.10 maks | 2 maks | 0.75 maks | 0.045 maks | 0.03 maks | 17 - 19 | 4xC min 0,60 % maks |
9 - 12 | 0.10 maks |
| SS 347 | 0.08 maks | 2 maks | 0.75 maks | 0.045 maks | 0.03 maks | 17 - 20 | 10xC min 1.00 maks |
9 - 13 | 62.74 |
| SS 347H | 0.04 – 0.10 | 2 maks | 0.75 maks | 0.045 maks | 0.03 maks | 17 - 20 | 8xC min 1.00 maks |
9 - 13 | 62.74 |
| SS 446 | 0.2 maks | 1,5 maks | 0.75 maks | 0.040 maks | 0.03 maks | 23 – 30 | 0.10 – 0.25 | 0.50 maks | Balansere |
Rustfritt stål smeltepunkt, tetthet og strekkstyrke
| Karakter | Tetthet | Smeltepunkt | Strekkstyrke | Yield Strength (0.2%Offset) | Forlengelse |
| SS 304 | 8.0 g/cm3 | 1400 grader (2550 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 35 % |
| SS 304L | 8.0 g/cm3 | 1400 grader (2550 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 40 % |
| SS 310 | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 35 % |
| SS 310S | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 35 % |
| SS 316 | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 35 % |
| SS 316L | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 40 % |
| SS 317 | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 35 % |
| SS 317L | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 35 % |
| SS 321 | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 35 % |
| SS 321H | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 35 % |
| SS 347 | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 40 % |
| SS 347H | 8.0 g/cm3 | 1454 grader (2650 grader F) | Psi – 75 000 , MPa – 515 | Psi – 30 000, MPa – 205 | 40 % |
| SS 446 | 7,5 g/cm3 | 1510 grader (2750 grader F) | Psi – 75,000 , MPa – 485 | Psi – 40,000 , MPa – 275 | 20 % |